Author:Väyrynen, Petri
Title:Levyaihioiden poikittaishalkeamiin vaikuttavat tekijät teräksen jatkuvavalussa
Influencing factors of transverse cracking of slabs in continuous casting of steel
Publication type:Master's thesis
Publication year:2004
Pages:94+3      Language:   fin
Department/School:Materiaali- ja kalliotekniikan osasto
Main subject:Metallurgia   (Mak-37)
Supervisor:Louhenkilpi, Seppo
Instructor:Palovaara, Tomi ; Rentola, Ismo
OEVS:
Electronic archive copy is available via Aalto Thesis Database.
Instructions

Reading digital theses in the closed network of the Aalto University Harald Herlin Learning Centre

In the closed network of Learning Centre you can read digital and digitized theses not available in the open network.

The Learning Centre contact details and opening hours: https://learningcentre.aalto.fi/en/harald-herlin-learning-centre/

You can read theses on the Learning Centre customer computers, which are available on all floors.

Logging on to the customer computers

  • Aalto University staff members log on to the customer computer using the Aalto username and password.
  • Other customers log on using a shared username and password.

Opening a thesis

  • On the desktop of the customer computers, you will find an icon titled:

    Aalto Thesis Database

  • Click on the icon to search for and open the thesis you are looking for from Aaltodoc database. You can find the thesis file by clicking the link on the OEV or OEVS field.

Reading the thesis

  • You can either print the thesis or read it on the customer computer screen.
  • You cannot save the thesis file on a flash drive or email it.
  • You cannot copy text or images from the file.
  • You cannot edit the file.

Printing the thesis

  • You can print the thesis for your personal study or research use.
  • Aalto University students and staff members may print black-and-white prints on the PrintingPoint devices when using the computer with personal Aalto username and password. Color printing is possible using the printer u90203-psc3, which is located near the customer service. Color printing is subject to a charge to Aalto University students and staff members.
  • Other customers can use the printer u90203-psc3. All printing is subject to a charge to non-University members.
Location:P1 Ark V80     | Archive
Keywords:steel
continuous casting
transverse cracking
teräs
jatkuvavalu
poikittaishalkeamat
Abstract (eng): The objective in this master's thesis was to analyze continuous casting machine's data, which is automatically recorded during the cast, and to find out causes of transverse cracking.
Concentration is especially on cracking at the end of the cast.

The theoretical part examines some elements, which most affect hot ductility of steel.
The most important factors of continuous casting machine affecting to slabs surface quality are also examined.
Introduction of measure equipment used in experimental part of the thesis (machinery to calculate mould's friction and scanning pyrometer) is made in this section.

In the experimental part some part of the data was analyzed statistically (concentration of elements and thickness of rolled slabs) and the other part visually through different diagrams.
Data from pyrometer was examined with both practices.

According to measurement data no definite reasons for transverse cracking were found.
Surface temperature was always over A3 -temperature in straightening, as it should be, and there was no correlation between friction measurements and cracking.
Steel's composition did not reveal any explanatory differences either.
However heat transfer calculations pointed out that transverse cracks in end of cast can be developed in interaction between 3. secondary cooling areas relatively powerful cooling intensity and coarse crystal structure in mould born depressions.
If this theory is correct, reduction of 3. secondary cooling area's minimum water volume can be recommend as work's summary, which probably requires change of nozzles.
Abstract (fin): Diplomityön tavoitteena oli löytää jatkuvavalukoneelta tallennetuista tiedoista selittäviä tekijöitä varsinkin valusarjojen lopussa esiintyville poikittaishalkeamille.

Kirjallisuusosassa tarkastellaan alkuaineiden vaikutuksia teräksen kuumasitkeyteen, joka vaikuttaa voimakkaasti halkeamien syntyherkkyyteen.
Tämän lisäksi käydään läpi tärkeimmät valunauhan pinnanlaatuun vaikuttavat prosessimuuttujat.
Valukoneen kokillin kitkaa mittaava laitteisto ja valettavan aihion pintalämpötiloja mittaava skannaava kaksiväripyrometri esitellään myös työn tässä osassa.

Kokeellisessa osassa aineistoa tutkittiin pääosin tilastollisesti (alkuainepitoisuudet, valssattujen levyjen paksuudet).
Prosessimuuttujia ja kitkatietoja tarkasteltiin kuvaajien perusteella visuaalisesti.
Lämpötilatietoja vertailtiin kummallakin tavalla.

Mittausaineiston perusteella mitään selkeitä syitä poikittaishalkeamien syntyyn ei löytynyt.
Oikaisussa pintalämpötilat olivat aina selkeästi A3 -lämpötilojen yläpuolella, kuten pitääkin, eikä kitkamittaus korreloinut selkeästi halkeamien kanssa.
Selittäviä eroja ei löytynyt teräksen analyysistakaan.
Kuitenkin tehdyt lämmönsiirtolaskelmat osoittivat, että poikittaishalkeamat voivat syntyä valun lopussa 3. toisiojäähdytysvyöhykkeen suhteellisen voimakkaan jäähdytystehon ja kokillissa syntyvien painaumien aiheuttaman karkean kiderakenteen yhteisvaikutuksesta.
Jos teoria pitää paikkansa, työn johtopäätöksenä voidaankin suositella minimivesimäärien vähentämistä 3. toisiojäähdytysvyöhykkeellä, mikä tosin edellyttänee suutinten vaihtamista.