Author:Forsberg, Miika Jani
Title:Kiinteistöjen metallisten käyttövesiputkistojen ja -laitteistojen kestävyys
Durability of household metallic water supply systems
Publication type:Master's thesis
Publication year:2009
Pages:113      Language:   fin
Department/School:Materiaalitekniikan laitos
Main subject:Vesihuoltotekniikka   (Yhd-73)
Supervisor:Vahala, Riku
Instructor:Aromaa, Jari ; Pääkkönen, Jorma
OEVS:
Electronic archive copy is available via Aalto Thesis Database.
Instructions

Reading digital theses in the closed network of the Aalto University Harald Herlin Learning Centre

In the closed network of Learning Centre you can read digital and digitized theses not available in the open network.

The Learning Centre contact details and opening hours: https://learningcentre.aalto.fi/en/harald-herlin-learning-centre/

You can read theses on the Learning Centre customer computers, which are available on all floors.

Logging on to the customer computers

  • Aalto University staff members log on to the customer computer using the Aalto username and password.
  • Other customers log on using a shared username and password.

Opening a thesis

  • On the desktop of the customer computers, you will find an icon titled:

    Aalto Thesis Database

  • Click on the icon to search for and open the thesis you are looking for from Aaltodoc database. You can find the thesis file by clicking the link on the OEV or OEVS field.

Reading the thesis

  • You can either print the thesis or read it on the customer computer screen.
  • You cannot save the thesis file on a flash drive or email it.
  • You cannot copy text or images from the file.
  • You cannot edit the file.

Printing the thesis

  • You can print the thesis for your personal study or research use.
  • Aalto University students and staff members may print black-and-white prints on the PrintingPoint devices when using the computer with personal Aalto username and password. Color printing is possible using the printer u90203-psc3, which is located near the customer service. Color printing is subject to a charge to Aalto University students and staff members.
  • Other customers can use the printer u90203-psc3. All printing is subject to a charge to non-University members.
Location:P1 Ark TKK  105   | Archive
Keywords:copper pipe
corrosion
pitting corrosion
potable water
water corrosiveness
silica
water treatment
kupariputki
korroosio
pistesyöpyminen
käyttövesi
veden syövyttävyys
silikaatti
veden käsittely
Abstract (eng): Groundwater facilities, excluding the smallest facilities, mitigate corrosion in water supply networks by alkalising raw water.
Despite raw water deacidification, pitting corrosion occurs in household water supply systems occasionally.
Corrosion is a result of several parameters.
Water quality, system design, installation, commissioning, maintenance and variation of water usage affect durability of household piping among others.

Anti-corrosive quality of copper and stainless steel in potable water supply systems is based on passivation of metal surfaces.
However, if passivation layer brakes down locally, pure metal surface is exposed.
Pure metal surface may become non-productive and pitting corrosion may occur.
In general, copper pitting is relatively rare phenomenon.

Two surveys were conducted: one for waterworks and one for households.
Based on waterworks survey, most copper corrosion incidents were observed in row houses, and in large public buildings such as schools and hospitals.
The household survey revealed that household water supply system problems occurred mainly as leaks in hot water boilers.

Five copper pipes with pitting corrosion damage were investigated.
Reasons for pitting failures were tried to be explained by water and copper pipe quality investigations.
Furthermore, one undamaged copper pipe was examined similarly.
The mam purpose of the field investigations was to clarify the possible role of silica film in copper pitting.

In some of field targets, water quality, particularly pH variation, was observed to have a possible role in pitting failures.
Water silicate concentration did not affect silica film formation inside copper tubes.

Water supply personnel are recommended to become aware of the role of water in electrochemical corrosion reaction and to undertake proactive actions to prevent corrosion in water supply network.
Abstract (fin): Pohjavesilaitoksilla, aivan pienimpiä lukuun ottamatta, raakavesi alkaloidaan jakeluverkoston korroosion estämiseksi.
Veden alkaloinnista huolimatta kiinteistöjen metallisten käyttövesiputkistojen ja -laitteistojen syöpymistä esiintyy aika ajoin.
Korroosioilmiöihin vaikuttavat monet eri muuttujat.
Veden laadun lisäksi mm. kiinteistön käyttövesijärjestelmien mitoitus, asennus, käyttöönotto ja käyttöolosuhdevaihtelut muodostavat niiden kestävyyden kannalta kriittiset vaiheet.

Kuparin ja ruostumattoman teräksen hyvä korroosionkestävyys käyttövesisovelluksissa perustuu metallin pinnalle muodostuvaan passivoivaan suojakerrokseen.
Jos suojakerros tuhoutuu paikallisesti, metalli altistuu sähkökemialliselle korroosiolle ja voi syöpyä puhki.
Kupariputken vaurioituminen pistekorroosiomekanismilla on verraten harvinaista.

Työssä tehtiin kaksi kyselytutkimusta: vesilaitoskysely ja kiinteistökysely.
Vesilaitoskyselyn perusteella vesilaitoksen toiminta-alueella eniten kuparin syöpymishavaintoja tehtiin rivitaloissa ja isoissa julkisissa rakennuksissa, kuten kouluissa ja sairaaloissa.
Kiinteistökyselyn perusteella kiinteistöjen käyttövesijärjestelmien ongelmat esiintyivät yleisimmin lämminvesivaraajien vuotoina.

Työssä tutkittiin viisi käytössä läpisyöpynyttä kupariputkea ja pyrittiin selvittämään vaurioitumiseen johtaneita syiltä veden laadun ja putkianalyysien avulla.
Lisaksi tutkittiin yksi vaurioitumaton kupariputki.
Kenttätutkimuskohteiden avulla selvitettiin mahdollisen silikaattikalvon roolia kupariputken pistesyöpymisessä.

Veden laadun, erityisesti pH-arvon vaihteluilla havaittiin olevan mahdollinen yhteys osaan tutkituista vaurioituneista kupariputkista.
Talousveden silikaattipitoisuus ei vaikuttanut siihen, muodostuiko vaurioituneen tai vaurioitumattoman kupariputken sisäpinnalle silikaattikalvo vai ei.

Vesilaitosten olisi suositeltavaa tiedostaa veden rooli sähkökemiallisen korroosion yhtenä osatekijänä ja ryhtyä sen johdosta ennakoiviin toimenpiteisiin metallisten verkosto-osien korroosion estämiseksi.
ED:2012-08-29