search query: @keyword liuotus / total: 13
reference: 6 / 13
« previous | next »
Author:Porvali, Antti
Title:Kullan liuotus tiosulfaatilla
Gold thiosulfate leaching
Publication type:Master's thesis
Publication year:2014
Pages:ix + 98 s. + liitt. 16      Language:   fin
Department/School:Materiaalitekniikan laitos
Main subject:Materiaalien prosessointi   (MT3002)
Supervisor:Forsén, Olof
Instructor:Kaartinen, Tommi ; Aromaa, Jari
Electronic version URL: http://urn.fi/URN:NBN:fi:aalto-201411223047
OEVS:
Electronic archive copy is available via Aalto Thesis Database.
Instructions

Reading digital theses in the closed network of the Aalto University Harald Herlin Learning Centre

In the closed network of Learning Centre you can read digital and digitized theses not available in the open network.

The Learning Centre contact details and opening hours: https://learningcentre.aalto.fi/en/harald-herlin-learning-centre/

You can read theses on the Learning Centre customer computers, which are available on all floors.

Logging on to the customer computers

  • Aalto University staff members log on to the customer computer using the Aalto username and password.
  • Other customers log on using a shared username and password.

Opening a thesis

  • On the desktop of the customer computers, you will find an icon titled:

    Aalto Thesis Database

  • Click on the icon to search for and open the thesis you are looking for from Aaltodoc database. You can find the thesis file by clicking the link on the OEV or OEVS field.

Reading the thesis

  • You can either print the thesis or read it on the customer computer screen.
  • You cannot save the thesis file on a flash drive or email it.
  • You cannot copy text or images from the file.
  • You cannot edit the file.

Printing the thesis

  • You can print the thesis for your personal study or research use.
  • Aalto University students and staff members may print black-and-white prints on the PrintingPoint devices when using the computer with personal Aalto username and password. Color printing is possible using the printer u90203-psc3, which is located near the customer service. Color printing is subject to a charge to Aalto University students and staff members.
  • Other customers can use the printer u90203-psc3. All printing is subject to a charge to non-University members.
Location:P1 Ark Aalto  2534   | Archive
Keywords:thiosulfate
gold
leaching
hydrometallurgy
electrochemistry
tiosulfaatti
kulta
liuotus
hydrometallurgia
esirikaste
sähkökemialliset kokeet
Abstract (eng):The conventional method of gold leaching is cyanide leaching, which is potentially dangerous to the environment.
Due to this danger there has been an increased interest in finding a new, environment friendly leaching process.
One of the more promising candidates has been thiosulfate leaching of gold.

In this thesis research over last thirty years was investigated.
In the literature work there are presented the basis of thiosulfate leaching of gold.
Reaction kinetics and thermodynamics of the leaching are covered.
Factors influencing the leaching process, such as reagents, additives, oxidizers and raw materials, were investigated.

The experimental part was divided to two parts: the first involving electrochemical experiments where pure gold was leached in potentiostatic control.
Electrochemical quartz microbalance was used as a working electrode.
Changing current densities and electrode masses were recorded as a function of time.
The parameters used in factor analysis were temperature, redox potential and ammonia concentration.
Based on the results of the electrochemical experiments the second part of the experimental work was planned.
The second part consisted of batch reactor tests where enriched, autoclaved sand was leached over 6 hours.
The reactor was made of glass and was 3 dm3 in volume.
Pulp densities of 10, 20 and 30 % were used in separate tests along with different mixing speeds.
The constant parameters were gas bubbling (500 cm3/min), temperature (30 °C), solution (0,6 M NH3, 0,01 M CuSO4, 0,4 Na2SO4, 0,2 Na2S2O3).
Samples were taken from the reactor in regular intervals.

The results of the first part of the experimental work were such that the maximum current reached was 1 mA/cm2.
At best, leaching achieved 2,98 mg/(h*cm2) with ammonium thiosulfate and 2,68 mg/(h*cm2) with sodium thiosulfate.
In batch reactor experiments the best yield was 88 %.
There was a distinct disappearance of gold after each batch reactor experiment.
The exact reason for this is unclear and further investigation is necessary.
Abstract (fin):Vallitseva kullan liuotusmenetelmä on syanidiliuotus, joka on potentiaalisesti ympäristölle vaarallinen liuotusmenetelmä.
Tämän vuoksi on etsitty syanidiliuotukselle vaihtoehtoja.
Yksi lupaavimmista vaihtoehdoista on ollut tiosulfaattiliuotus.

Tässä työssä perehdyttiin kullan tiosulfaattiliuotuksen teoriaan viimeisen kolmenkymmenen vuoden tutkimuksen puolesta.
Työn kirjallisessa osiossa esitetään liuotukseen perusteita ja liuotukseen vaikuttavia tekijöitä.
Liuotuksen reaktiokinetiikkaan ja termodynamiikkaan perehdyttiin kirjallisuuden avulla.
Perehdyttiin liuotukseen vaikuttaviin seikkoihin, kuten reagenssien, additiivien, hapettimien ja raaka-aineiden vaikutukseen.

Kokeellinen osio oli jaettu kahteen osaan: sähkökemiallisissa kokeissa tutkittiin liuotuksen edellytyksiä potentiostaattisten kokeiden avulla faktorianalyysina.
Käyttäen kvartsikidemikrovaakaa työelektrodina ja potentiostaattia, mitattiin liuotuksessa massan muutosta ja virrantiheyttä ajan funktiona.
Faktorikokeen muuttuvana parametrina oli lämpötila, redox-potentiaali ja ammoniakkikonsentraatio.
Tulosten perusteella suunniteltiin jälkimmäinen kokeellinen puolisko, jossa liuotettiin kaivokselta saatua esirikastetta reaktorikokeissa.
Reaktorikokeissa esirikastetta liuotettiin 3L reaktorissa 10, 20, ja 30 % kiintoainespitoisuuksilla.
Vakiomuuttujina olivat kuplitus (500 cm3/min), lämpötila (30 °C), liuos (0,6 M NH3, 0,01 M CuSO4, 0,4 Na2SO4, 0,2 Na2S2O3) Reaktorista otettiin ennalta määritellyin ajoin ruiskusuodatettuja näytteitä noin 10 ml.
Reaktorikokeiden jälkeen liuokset ja liuotusjäännökset kuivattiin, jauhettiin ja pussitettiin kahdeksaan osaan.

Sähkökemiallisten kokeiden osalta päästiin enintään 1 mA/cm2 virrantiheyteen.
Liuotusnopeuksien puolesta päästiin ammoniumtiosulfaatilla maksimissaan 2,98 mg/(h*cm2) ja natriumtiosulfaatilla 2,68 mg/(h*cm2).
Reaktorikokeissa saannot jäivät parhaimmillaan 88 %, kun saanto laskettiin liuotuksessa olleen kiintoaineksen kultapitoisuuden perusteella.
Kullan analytiikassa oli ongelmia, joka näkyi noin 20 mg / kg kullan häviönä liuotuksen ja analyysin välissä.
Syy tälle jäi epäselväksi, ja jatkotutkimukset ovat tarpeen.