Author:Niiranen, Sini
Title:Plasmakäsitellyn nestekidepolymeerin ja silikonin välisen adheesion heikkeneminen kiihdytetyissä ympäristörasitustesteissä
Weakening of the adhesion between plasma treated liquid crystal polymer and silicone under accelerated environmental stress tests
Publication type:Master's thesis
Publication year:2011
Pages:[7] + 62      Language:   fin
Department/School:Elektroniikan laitos
Main subject:Elektroniikan valmistustekniikka   (S-113)
Supervisor:Paulasto-Kröckel, Mervi
Instructor:Turunen, Markus
Electronic version URL: http://urn.fi/URN:NBN:fi:aalto-201207022640
OEVS:
Electronic archive copy is available via Aalto Thesis Database.
Instructions

Reading digital theses in the closed network of the Aalto University Harald Herlin Learning Centre

In the closed network of Learning Centre you can read digital and digitized theses not available in the open network.

The Learning Centre contact details and opening hours: https://learningcentre.aalto.fi/en/harald-herlin-learning-centre/

You can read theses on the Learning Centre customer computers, which are available on all floors.

Logging on to the customer computers

  • Aalto University staff members log on to the customer computer using the Aalto username and password.
  • Other customers log on using a shared username and password.

Opening a thesis

  • On the desktop of the customer computers, you will find an icon titled:

    Aalto Thesis Database

  • Click on the icon to search for and open the thesis you are looking for from Aaltodoc database. You can find the thesis file by clicking the link on the OEV or OEVS field.

Reading the thesis

  • You can either print the thesis or read it on the customer computer screen.
  • You cannot save the thesis file on a flash drive or email it.
  • You cannot copy text or images from the file.
  • You cannot edit the file.

Printing the thesis

  • You can print the thesis for your personal study or research use.
  • Aalto University students and staff members may print black-and-white prints on the PrintingPoint devices when using the computer with personal Aalto username and password. Color printing is possible using the printer u90203-psc3, which is located near the customer service. Color printing is subject to a charge to Aalto University students and staff members.
  • Other customers can use the printer u90203-psc3. All printing is subject to a charge to non-University members.
Location:P1 Ark Aalto  1216   | Archive
Keywords:adhesion
weakening
silicone
plasma treatment
environmental stress test
adheesio
heikkeneminen
LCP
silikoni
plasmakäsittely
ympäristörasitustesti
Abstract (eng): The focus of this work was in the weakening of adhesion between plasma pretreated liquid crystal polymer (LCP) and silicone adhesive under environmental stress tests.
The use of polymers has been growing as a electronics manufacturing material.
Improving the adhesion between the polymers is one of the major challenges in the electronics manufacturing.
In this work adhesion mechanisms between polymers were studied as well as polymer surface pretreatments.
Environmental stresses, stress tests and their use in electronics reliability testing were covered in this work.
Adhesion weakening mechanisms under stress were also studied.

VTI Technologies supplied the research materials, silicone adhesive and Vectra liquid crystal polymer, for this work.
Materials are used in acceleration sensor manufacturing.
The component package was made of liquid crystal polymer and the surface was pretreated with plasma before silicone adhesive was dispensed on the surface.
The surface of the LCP was analyzed with sessile drop test, profilometer and X-ray photoelectron and infrared spectroscopy.
Some differences on the surface of the LCP were found after oxygen and argon based plasma treatments.

Wetting properties and surface roughness changed during the pretreatments.
There were also chemical changes in the LCP surface depending on the the plasma process gas.
Adhesion between the LCP and the silicone was measured with shear strength tester.
Pretreatments improved the adhesion significantly.

Environmental stress tests focused on humidity, temperature and the effect of corrosion gases.
The samples were placed in elevated temperatures and under corrosion gases as well as in different temperature and humidity tests.
The main cause of weakening of the adhesion was humidity.
Water molecules can penetrate the interface and disrupt the hydrogen bonds existing over the interface.
Elevated temperature improved the interface adhesion strength by dehydrating the interface and reconstructing the hydrogen bonds.
Corrosion gases enhanced the crosslinking in the silicone, but for the weakening of the adhesion they had a limited role.
Abstract (fin): Työssä tutkittiin plasmaesikäsitellyn nestekidepolymeerin (LCP) ja silikoniliiman välisen adheesion heikkenemistä ympäristörasitustesteissä.
Polymeerien käyttö on lisääntynyt jatkuvasti elektroniikan valmistusmateriaalina.
Polymeerien välisen adheesion parantaminen on yksi suurista haasteista elektroniikan valmistuksessa.

Tässä työssä tutkittiin polymeerien välisen adheesion mekanismeja ja polymeerien esikäsittelyä.
Työssä käytiin myös läpi erilaisia ympäristörasitusmenetelmiä ja niiden käyttöä elektroniikan luotettavuuden testauksessa.
Lisäksi työssä tutkittiin adheesion heikkenemismekanismeja, jotka johtuvat ympäristörasituksista.

VTI Technologies:n toimittamat tutkimusmateriaalit, eli silikoniliima ja Vectra- nestekidepolymeeri, ovat erään kiihtyvyysanturin valmistusmateriaaleja.
Nestekidepolymeeristä valmistetun komponenttikotelon pintaa esikäsiteltiin erilaisilla plasmakäsittelyillä, ennen kuin silikoniliima levitettiin LCP:n pinnalle.
LCP:n pintaa analysoitiin kontaktikulmamittauksien, profilometrin sekä röntgenfotoelektroni- ja infrapunaspektroskopian avulla.
LCP:n pinnassa havaittiin eroja happi- ja argonkaasuilla suoritettujen plasmakäsittelyiden jälkeen.
Pinnan kostutusominaisuudet ja karheus muuttuivat esikäsittelyjen aikana.
Pinnassa tapahtui myös kemiallisia muutoksia riippuen käytettävästä plasmakaasusta.
Adheesiota LCP:n ja silikonin välillä mitattiin leikkauslujuustestillä eli työntötestillä.
Esikäsittelyt paransivat adheesiota merkittävästi.

Ympäristörasitustesteissä keskityttiin kosteuden, lämpötilan ja korroosiokaasujen vaikutukseen.
Näytteitä asetettiin korotettuun lämpötilaan ja korroosiotestiin sekä erilaisiin lämpötila- ja kosteuspitotesteihin.
Adheesiota eniten heikentävä rasitus oli kosteus.
Vesimolekyylit tunkeutuvat rajapinnalle ja häiritsevät rajapinnan yli olevia vetysidoksia.
Korotettu lämpötila paransi adheesion voimakkuutta kuivattamalla rajapintaa ja mahdollisti vetysidosten uudelleenmuodostumisen.
Korroosiokaasut silloittivat silikonia edelleen, mutta adheesion voimakkuudelle niillä oli vähäinen merkitys.