Author:Jääskeläinen, Juha Matti
Title:Synthesis of thermally curable monomers for phenol-formaldehyde thermosets - their use and production optimization
Termisesti kovettuvien monomeerien synteesi fenoli-formaldehydipolymeereille - niiden käyttö ja valmistuksen optimointi
Publication type:Master's thesis
Publication year:2012
Pages:x + 88      Language:   eng
Department/School:Kemian laitos
Main subject:Orgaaninen kemia   (Kem-4)
Supervisor:Jokela, Reija
Instructor:Paulasaari, Jyri
OEVS:
Electronic archive copy is available via Aalto Thesis Database.
Instructions

Reading digital theses in the closed network of the Aalto University Harald Herlin Learning Centre

In the closed network of Learning Centre you can read digital and digitized theses not available in the open network.

The Learning Centre contact details and opening hours: https://learningcentre.aalto.fi/en/harald-herlin-learning-centre/

You can read theses on the Learning Centre customer computers, which are available on all floors.

Logging on to the customer computers

  • Aalto University staff members log on to the customer computer using the Aalto username and password.
  • Other customers log on using a shared username and password.

Opening a thesis

  • On the desktop of the customer computers, you will find an icon titled:

    Aalto Thesis Database

  • Click on the icon to search for and open the thesis you are looking for from Aaltodoc database. You can find the thesis file by clicking the link on the OEV or OEVS field.

Reading the thesis

  • You can either print the thesis or read it on the customer computer screen.
  • You cannot save the thesis file on a flash drive or email it.
  • You cannot copy text or images from the file.
  • You cannot edit the file.

Printing the thesis

  • You can print the thesis for your personal study or research use.
  • Aalto University students and staff members may print black-and-white prints on the PrintingPoint devices when using the computer with personal Aalto username and password. Color printing is possible using the printer u90203-psc3, which is located near the customer service. Color printing is subject to a charge to Aalto University students and staff members.
  • Other customers can use the printer u90203-psc3. All printing is subject to a charge to non-University members.
Location:P1 Ark Aalto  1975   | Archive
Keywords:novolac
WPL
RDL
4-hydroxyphenylmaleimide
novolakka
4-hydroksifenyylimaleimidi
Abstract (eng): The objective for this master's thesis was to investigate various options for functionalized monomers as part of thermosetting phenol-formaldehyde polymers.
The purpose was to chart, how the suitability of a polymer can be affected through monomer functionalization as packaging material for microchips.
The work was carried out at Silecs Oy, as part of their advanced packaging project.
The purpose of monomer charting was to find alternatives to the synthesis of the existing product for this application and reducing the complexity of the process.

In the survey part of the thesis, phenol-formaldehyde polymers their history, production and properties are introduced.
Additionally, the application for the product is described photo dielectric -including the requirements for the material and competing approaches.
Finally, the possible approaches for polymer functionalization are presented and the choice for monomer synthesis to be executed is revealed.

The experimental part of the thesis can be divided into three portions the monomer synthesis, polymer preparation and testing of the polymers.
The first part concentrates on 4-hydroxyphenylmaleimide and how it can be synthesized.
The second part describes how the above monomer can be used in preparation of three different types of polymers.
The third part explains how the polymers were tested and how the new polymers compare to the existing product in the required areas.

The results show, that the 4-hydroxyphenylmaleimide clearly enhances the chemical resistance of the polymer, without sacrificing physical properties.
The newly manufactured polymers had no increase in intrinsic stress because of the additional cross-linking, nor the polymers have a glass transition temperature below 200 °C.
However, the newly manufactured polymers had worse thermal resistance and patternability than the already optimized current product.
Abstract (fin): Tämän diplomityön tavoitteena oli tutkia eri vaihtoehtoja funktionaalisille monomeereille lämpökovetteisiin fenoli-formaldehydipolymeereihin.
Tarkoituksena on kartoittaa, kuinka monomeerien kautta voidaan vaikuttaa polymeerin soveltuvuuteen mikrosirujen paketointiaineena.
Työ toteutettiin Silecs Oy:lle osana kehittyneiden paketointimenetelmien projektia.
Kartoituksen avulla pyrittiin löytämään vaihtoehtoja olemassa olevalle tuotteelle ja siten valmistus prosessin yksinkertaistamiseen.

Työn teoria osuudessa käydään läpi fenoli-formaldehydipolymeerien historia, valmistus, tyypilliset ominaisuudet ja käyttö.
Lisäksi esitellään aiheena olevan polymeerin käyttökohde - fotokuvioitava, dielektrinen kerros - tälle vaadittavine ominaisuuksineen ja kilpailevine lähestymistapoineen.
Lopuksi kuvataan, kuinka polymeerejä voidaan funktionalisoida ja esitetään, minkälainen monomeeri valitaan käytettäväksi.

Työn kokeellinen osio jakautuu kolmeen osaan - monomeerien valmistukseen, polymeerien valmistukseen ja polymeerien testaukseen.
Näissä osissa kuvataan, kuinka 4-hydroksifenyylimaleimidiä voidaan synteettisesti valmistaa, kuinka tätä monomeeriä voidaan käyttää kolmen eri tavalla valmistetun polymeerin ja kuinka valmistetut polymeerit vertautuvat olemassa olevaan tuotteeseen vaadituilla osa-alueilla.

Tulokset osoittavat, että 4-hydroksifenyylimaleimidi lisää selvästi polymeerin kemikaalista kestävyyttä, ilman että fysikaaliset ominaisuudet karsivat.
Valmistettujen polymeerien aiheuttama sisäinen stressi el kasvanut polymeerin ristisilloittumisen aikana, eikä polymeerillä ollut lasiutumislämpötilaa ainakaan ennen 200 °C lämpötilaa.
Kuitenkin, valmistetut polymeerit kestivät lämpöä huonommin kuin olemassa oleva tuote.
Lisäksi, olemassa olevan tuotteen prosessoitavuus ja kuvioitavuus oli vielä parempaa kuin optimoimattomien uusien polymeerien.