| Author: | Fält, Teppo |
| Title: | Mechanical properties of advanced ceramic coatings grown by thermal spraying |
| Publication type: | Master's thesis |
| Publication year: | 2005 |
| Pages: | 62 Language: eng |
| Department/School: | Materiaalitekniikan osasto |
| Main subject: | Metalli- ja materiaalioppi (Mak-45) |
| Supervisor: | Hannula, Simo-Pekka |
| Instructor: | Turunen, Erja |
| OEVS: | Electronic archive copy is available via Aalto Thesis Database.
Instructions Reading digital theses in the closed network of the Aalto University Harald Herlin Learning CentreIn the closed network of Learning Centre you can read digital and digitized theses not available in the open network. The Learning Centre contact details and opening hours: https://learningcentre.aalto.fi/en/harald-herlin-learning-centre/ You can read theses on the Learning Centre customer computers, which are available on all floors.
Logging on to the customer computers
Opening a thesis
Reading the thesis
Printing the thesis
|
| Location: | P1 Ark TKK 72 | Archive |
| Keywords: | thermal spraying high-velocity oxy-fuel HVOF ceramic coatings mechanical characterisation nanoindentation terminen ruiskutus suurnopeusliekkiruiskutus HVOF keraamiset pinnoitteet mekaaninen karakterisointi nanoindentaatio |